An order of steel mesh reinforced PE pipes and electro fusion fittings was delivered

This order was delivered on Jan.5th, 2019. ITEM DESCRIPTION OF GOODS QUANTITY 1 steel mesh reinfocced polyethylene pipe (smr-PE),110mm outer dia,PN-16 6000 2 steel mesh reinfocced polyethylene pipe (smr-PE),75mm outer dia,PN-16 3000 3 SMR-PE-pipe,50mm OD PN-16 4000 4 SMR-PE-pipe,25mm OD PN-16 4000 5 SMR-PE-jointing Machine for 25mm to 160mm pipe jointing 1 6 SMR-PE-Coupler,110mm CO,PN16 900 7 SMR-PE-‘T’,110mm OD,PN16 20 8 SMR-PE-Bend 90°,110mm CO PN-16 30 9 SMR-PE Bend 45°,110mm OD PN-16 20 10 SMR-PE Elbow,110mm OD,PN16 20 11 SMR-PE-Reducer form 110mm OD to 75mmOD,PN-16 20 12 SMR-PE-Reduter form 110mm OD,to 50mm OD,PN-16 15 13 SMR-PE-Reduter form 110 OD to 25mm OD 10 14 SMR-PE-Matching flanges with nut bolts,110mm OD,PN-16 60 15 SMR-PE-Coupler 75mm outer Dia 750…

S355J0 – BS EN 10025-2:2004

S355J0 BS EN 10025-2:2004 Hot rolled products of structural steels Part 2: Technical delivery conditions for non-alloy structural steels Chemical composition of the ladle analysis of S355J0 Chemical composition of the prduct analysis of S355J0 Maximum CEV based on the ladle analysis of S355J0 Mechanical properties of S355J0 impact strength KV longitudinal S355J0  

ASTM A182 F904L

ASTM A 182 Forged or Rolled Alloy and Stainless Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service Grade F904L (Austenitic Stainless Steels) Chemical Requirements: Composition, %, max C: 0.020 Mn:2.00 P: ≤0.040 S: ≤0.030 Si: 1.00 Cr: 19.0-23.0 Ni:23.0-28.0 Mo: 4.0-5.0 Cu:1.00-2.00 N: 0.10 Austenitizing/Solutioning Temperature: 1040 °C – 1150℃ Cooling Media: Liquid Quenching Cool Below ℃ 260…

ASTM A 182 F48

ASTM A 182 Forged or Rolled Alloy and Stainless Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service Grade F48 (Austenitic Stainless Steels) Chemical Requirements: Composition, %, max C: 0.030 Mn:2.00 P: ≤0.045 S: ≤0.030 Si: 0.75 Cr: 17.0-20.0 Ni:13.5-17.5 Mo: 4.0-5.0 N: 0.10-0.20 Austenitizing/Solutioning Temperature, min: 1040 °C Cooling Media: Liquid Quenching Cool Below ℃ 260 Tensile…

A312 UNS N08904

ASTM A 312 Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes UNS Designation N08904 Chemical Requirements: Composition, %, max C: 0.020 Mn:2.00 P: ≤0.040 S: ≤0.030 Si: 1.00 Cr: 19.0-23.0 Ni:23.0-28.0 Mo: 4.0-5.0 N: 0.10 Cu: 1.00-2.00   Heat Treating Temperature: 1100 °C   Tensile Requirements Tensile Strength, min.: 490MPa Yield Strength, min.: 215MPa Elongation in 2…

A312 UNS S31726

ASTM A 312 Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes UNS Designation S31726 Chemical Requirements: Composition, %, max C: 0.03 Mn:2.00 P: ≤0.040 * S: ≤0.030 Si: 1.00 Cr: 17.0-20.0 Ni:14.5-17.5 Mo: 4.0-5.0 N: 0.10-0.20 Cu: 0.75 *For welded pipe, the phosphorus maximum shall be 0.045 %. Heat Treating Temperature: 1040 °C Tensile Requirements Tensile Strength,…