BS3692:2001

BS 3692:2001 ISO metric precision hexagon bolts, screws and nuts – Specification BS3692 gives the general dimensions and tolerances of precision hexagon bolts, screws and nuts with ISO metric threads in diameters from 1.6mm to 68mm inclusive. Mechanical properties are given only in respect of carbon or alloy steel bolts, screws and nuts, which are not…

30ХГСА-GOST 4543

Standard: GOST 4543 Steel Grade: 30ХГСА Chemical Requirements  Composition, max, % Elements 30ХГСА Carbon 0.28-0.34 Silicon 0.90-1.20 Manganese 0.80-1.10 Chromium 0.80-1.10 Phosphorus 0.025 Sulfur 0.025 Copper 0.30 Nickel 0.30   Tensile, Impact and Hardness Requirements Steel Grade 30ХГСА Yield Strength, min, N/mm2 835 Ultimate Strength,min, N/mm2 1080 Elongation, min, % 10 Contraction, min, % 45 Shock viscosity…

INCONEL® 625

INCONEL® 625 is a nonmagnetic, corrosion and oxidation resistant, nickel-base alloy. It has high strength and toughness in the temperature range cryogenic to 2000°F (1093°C) which is derived largely from the solid solution effects of the refractory metals, columbium and molybdenum, in a nickel-chromium matrix. Alloy 625 has excellent fatigue strength and stress-corrosion cracking resistance…

40X GOST 4543

Standard: GOST 4543 Steel Grade: 40X Chemical Requirements  Composition, max, % Elements 40X – GOST 4543 Carbon 0.36 – 0.44 Silicon 0.17 – 0.37 Manganese 0.50 – 0.80 Chromium 0.80 – 1.10 Phosphorus 0.035 Sulfur 0.035 Copper 0.30 Nickel 0.30   Tensile, Impact and Hardness Requirements Steel Grade 40X – GOST 4543 Yield Strength, min,…

GOST 4543

GOST 4543 Alloyed Construciton Steel Gost 4543 applies to alloyed construction hot-rolled and forged gauged steel with diameter or thickness up to 250 mm, and steel with a special surface finish, used in a thermally treated condition and produced in the form of bars, strips and hanks. Regarding the standards for chemical composition this Standard…

ASME B16.21

ASME B16.21 NONMETALLIC FLAT GASKETS FOR PIPE FLANGES ASME B16.21 covers types, sizes, materials, dimensions, tolerances, and markings for nonmetallic flat gaskets. These gaskets are dimensionally suitable for use with flanges described in the referenced flange standards. Gasket Marking Gaskets shall be packaged with NPS, Class, gasket manufacturer’s name, material designation, thickness, and ASME B16.21 marked…

ASME B16.20

ASME B16.20 METALLIC GASKETS FOR PIPE FLANGES Ring-Joint, Spiral-Wound, and Jacketed ASME B16.20 covers materials, dimensions, tolerances, and markings for metal ring-joint gaskets, spiral wound metal gaskets,and metal-jacketed gaskets.These gaskets are dimensionally suitable for use with flanges described in reference flange standards ASME B16.5, ASMEB16.47, API Specification 6A, and ISO 10423. This Standard covers spiral-wound metal…

ASTM A312

ASTM A312 – Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes This specification covers seamless, straight-seam welded, and heavily cold worked welded austenitic stainless steel pipe intended for high-temperature and general corrosive service. The pipe shall be manufactured by one of the following processes: 1) Seamless (SML) pipe shall be made by a…

A182 F60

Identification Symbol: A182 F60 UNS Designation: S32205 Type: Ferritic – Austenitic Stainless Steel Heat Treatment: Solution Treat and Quench   Chemical Requirements  Composition, max, % Elements A182 F60 Carbon 0.030 Manganese 1.50 Phosphorus 0.030 Sulfur 0.020 Silicon 1.00 Nickel 4.5-6.5 Chromium 22.0-23.0 Molybdenum 3.0-3.5 Nitrogen 0.14-0.20   Tensile and Hardness Requirements Grade Symbol F60 Tensile Strength,min,…

St35.8 and St45.8

Standard: DIN 17175 Grade: St35.8, St45.8 Chemical composition Elements St35.8 (1.0305) St45.8 (1.0405) C ≤0.17 ≤0.21 Si 0.1-0.35 0.1-0.35 Mn 0.40-0.80 0.40-1.20 P  max 0.040 0.040 S  max 0.040 0.040   Mechanical properties Steel grade Tensile properties at room temperature Impact properties Upper yield stength or proof strength ReH or RP0.2 for Wall Thickness T…