ASTM A312 TP316L

ASTM A312 TP316L Chemical Requirements:  Composition, %, max Grade TP316L(S31603) Carbon 0.035 a Manganese 2.00 Phosphorus 0.045 Sulfur 0.030 Silicon 1.00 Chromium 16.0-18.0 Nickel 11.0-14.0 Molybdenum 2.00-3.00 a For small diameter or thin walls or both, where many drawing passes are required, a carbon maximum of 0.040 % is necessary in grades TP304L and TP316L. Small outside…

ASTM A312 TP316

ASTM A312 TP316 Chemical Requirements:  Composition, %, max Grade TP316(S31600) Carbon 0.08 Manganese 2.00 Phosphorus 0.045 Sulfur 0.030 Silicon 1.00 Chromium 16.0-18.0 Nickel 11.0-14.0 a Molybdenum 2.00-3.00 a For welded TP316 pipe, the nickel range shall be 10.0–14.0 %.   Heat Treating Temperature: 1900 °F [1040 °C]   Tensile Requirements: Tensile Strength, min ksi [MPa] 75 [515]…

ASTM A312 304H

ASTM A312 TP304H Chemical Requirements:  Composition, %, max Grade TP304H(S30409) Carbon 0.04-0.10 Manganese 2.00 Phosphorus 0.045 Sulfur 0.030 Silicon 1.00 Chromium 18.0-20.0 Nickel 8.0-11.0   Heat Treating Temperature:  Cold finished 1900 °F [1040 °C] Hot finished 1900 °F [1040 °C]   Tensile Requirements: Tensile Strength, min ksi [MPa] 75 [515] Yield Strength, min ksi [MPa] 30…

ASTM A312 TP304L

ASTM A312 TP304L Chemical Requirements:  Composition, %, max Grade TP304L(S30403) Carbon 0.035 a Manganese 2.00 Phosphorus 0.045 Sulfur 0.030 Silicon 1.00 Chromium 18.0-20.0 Nickel 8.0-13.0 a For small diameter or thin walls or both, where many drawing passes are required, a carbon maximum of 0.040 % is necessary in grades TP304L and TP316L. Small outside diameter tubes…

ASTM A312 TP304

ASTM A312 TP304 Chemical Requirements:  Composition, %, max Grade TP304(S30400) Carbon 0.08 Manganese 2.00 Phosphorus 0.045 Sulfur 0.030 Silicon 1.00 Chromium 18.0-20.0 Nickel 8.0-11.0   Heat Treating Temperature: 1900 °F [1040 °C] Tensile Requirements: Tensile Strength, min ksi [MPa] 75 [515] Yield Strength, min ksi [MPa] 30 [205] Elongation in 2 in. or 50 mm (or 4D),…

30ХГСА-GOST 4543

Standard: GOST 4543 Steel Grade: 30ХГСА Chemical Requirements  Composition, max, % Elements 30ХГСА Carbon 0.28-0.34 Silicon 0.90-1.20 Manganese 0.80-1.10 Chromium 0.80-1.10 Phosphorus 0.025 Sulfur 0.025 Copper 0.30 Nickel 0.30   Tensile, Impact and Hardness Requirements Steel Grade 30ХГСА Yield Strength, min, N/mm2 835 Ultimate Strength,min, N/mm2 1080 Elongation, min, % 10 Contraction, min, % 45 Shock viscosity…

INCONEL® 625

INCONEL® 625 is a nonmagnetic, corrosion and oxidation resistant, nickel-base alloy. It has high strength and toughness in the temperature range cryogenic to 2000°F (1093°C) which is derived largely from the solid solution effects of the refractory metals, columbium and molybdenum, in a nickel-chromium matrix. Alloy 625 has excellent fatigue strength and stress-corrosion cracking resistance…

40X GOST 4543

Standard: GOST 4543 Steel Grade: 40X Chemical Requirements  Composition, max, % Elements 40X – GOST 4543 Carbon 0.36 – 0.44 Silicon 0.17 – 0.37 Manganese 0.50 – 0.80 Chromium 0.80 – 1.10 Phosphorus 0.035 Sulfur 0.035 Copper 0.30 Nickel 0.30   Tensile, Impact and Hardness Requirements Steel Grade 40X – GOST 4543 Yield Strength, min,…

A182 F60

Identification Symbol: A182 F60 UNS Designation: S32205 Type: Ferritic – Austenitic Stainless Steel Heat Treatment: Solution Treat and Quench   Chemical Requirements  Composition, max, % Elements A182 F60 Carbon 0.030 Manganese 1.50 Phosphorus 0.030 Sulfur 0.020 Silicon 1.00 Nickel 4.5-6.5 Chromium 22.0-23.0 Molybdenum 3.0-3.5 Nitrogen 0.14-0.20   Tensile and Hardness Requirements Grade Symbol F60 Tensile Strength,min,…

St35.8 and St45.8

Standard: DIN 17175 Grade: St35.8, St45.8 Chemical composition Elements St35.8 (1.0305) St45.8 (1.0405) C ≤0.17 ≤0.21 Si 0.1-0.35 0.1-0.35 Mn 0.40-0.80 0.40-1.20 P  max 0.040 0.040 S  max 0.040 0.040   Mechanical properties Steel grade Tensile properties at room temperature Impact properties Upper yield stength or proof strength ReH or RP0.2 for Wall Thickness T…