INCONEL® 600

Inconel® 600 Equivalent designations UNS N06600 DIN W. Nr. 2.4816   Form ASTM Rod, bar and wire B 166 Plate, sheet and strip B 168, B 906 Seamless pipe and tube B 167, B 829 Welded pipe B 517, B 775 Welded tube B 516, B 751 Welding fitting B 366 Billet and bar for…

ASTM A516 GR70

ASTM A516 – Pressure Vessel Plates, Carbon Steel, for Moderate- and Lower-Temperature Service Grade: 70   Chemical Requirements Elements Grade70[485] Carbon,max A,B:     1⁄2 in. [12.5 mm] and under 0.27     Over 1⁄2 in. to 2 in. [12.5 to 50 mm], incl 0.28     Over 2 in. to 4 in. [50 to 100 mm], incl 0.30…

ASTM A516 GR65

ASTM A516 – Pressure Vessel Plates, Carbon Steel, for Moderate- and Lower-Temperature Service Grade: 65   Chemical Requirements Elements Grade65[450] Carbon,max A,B:     1⁄2 in. [12.5 mm] and under 0.24     Over 1⁄2 in. to 2 in. [12.5 to 50 mm], incl 0.26     Over 2 in. to 4 in. [50 to 100 mm], incl 0.28…

ASTM A516 GR60

ASTM A516 – Pressure Vessel Plates, Carbon Steel, for Moderate- and Lower-Temperature Service Grade: 60   Chemical Requirements Elements Grade60[415] Carbon,max A,B:     1⁄2 in. [12.5 mm] and under 0.21     Over 1⁄2 in. to 2 in. [12.5 to 50 mm], incl 0.23     Over 2 in. to 4 in. [50 to 100 mm], incl 0.25…

ASTM A516 GR55

ASTM A516 – Pressure Vessel Plates, Carbon Steel, for Moderate- and Lower-Temperature Service Grade: 55   Chemical Requirements Elements Grade55[380] Carbon,max A,B:     1⁄2 in. [12.5 mm] and under 0.18     Over 1⁄2 in. to 2 in. [12.5 to 50 mm], incl 0.20     Over 2 in. to 4 in. [50 to 100 mm], incl…

ASTM A36-Plates

Plates –  ASTM A36 Carbon Structural Steel Chemical Requirements: Product Plates A                                Thickness, in. [mm]                      To 3⁄4[20],incl     Over 3⁄4 to     1- ⁄2 [20 to 40],incl Over…

ASTM A36 -Shapes

Shapes – ASTM A36 Carbon Structural Steel Chemical Requirements: Product Shapes A Thickness, in. [mm] All Carbon, max, % 0.26 Manganese, % – Phosphorus, max, % 0.04 Sulfur, max, % 0.05 Silicon, % 0.40 max. Copper, min, % when copper steel is specified 0.20 A Manganese content of 0.85–1.35 % and silicon content of 0.15–0.40…

ASTM A312 TP347

ASTM A312 TP347 Chemical Requirements:  Composition, %, max Grade TP347(S34700) Carbon 0.08 Manganese 2.00 Phosphorus 0.045 Sulfur 0.030 Silicon 1.00 Chromium 17.0-19.0 Nickel 9.0-13.0 Columbium 10*Carbon-1.00   Heat Treating Temperature: 1900 °F [1040 °C]   Tensile Requirements: Tensile Strength, min ksi [MPa] 75 [515] Yield Strength, min ksi [MPa] 30 [205]   Elongation in 2 in. or…

ASTM A312 TP321

ASTM A 312 Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes Grade: TP321 UNS Designation:: S32100 Chemical Requirements(%): C: ≤0.08 Mn: ≤2.00 P: ≤0.045 S: ≤0.030 Si: ≤1.00 Cr: 17.0-19.0 Ni: 9.0-12.0 Ti: 5×(C+N)-0.70 N: ≤0.10 Heat Treating Temperature: Solution, ≥1040 °C Tensile Requirements: For welded pipe, Tensile Strength, ≥515Mpa Yield Strength, ≥205MPa For seamless…

ASTM A312 TP316H

ASTM A312 TP316H Chemical Requirements:  Composition, %, max Grade TP316H(S31609) Carbon 0.04-0.10 Manganese 2.00 Phosphorus 0.045 Sulfur 0.030 Silicon 1.00 Chromium 16.0-18.0 Nickel 11.0-14.0 a Molybdenum 2.00-3.00 a For welded TP316H pipe, the nickel range shall be 10.0–14.0 %.   Heat Treating Temperature:  Cold finished 1900 °F [1040 °C] Hot finished 1900 °F [1040 °C]  …