ASTM A312 TP316L

ASTM A312 TP316L Chemical Requirements:  Composition, %, max Grade TP316L(S31603) Carbon 0.035 a Manganese 2.00 Phosphorus 0.045 Sulfur 0.030 Silicon 1.00 Chromium 16.0-18.0 Nickel 11.0-14.0 Molybdenum 2.00-3.00 a For small diameter or thin walls or both, where many drawing passes are required, a carbon maximum of 0.040 % is necessary in grades TP304L and TP316L. Small outside…

ASTM A312 TP316

ASTM A312 TP316 Chemical Requirements:  Composition, %, max Grade TP316(S31600) Carbon 0.08 Manganese 2.00 Phosphorus 0.045 Sulfur 0.030 Silicon 1.00 Chromium 16.0-18.0 Nickel 11.0-14.0 a Molybdenum 2.00-3.00 a For welded TP316 pipe, the nickel range shall be 10.0–14.0 %.   Heat Treating Temperature: 1900 °F [1040 °C]   Tensile Requirements: Tensile Strength, min ksi [MPa] 75 [515]…

ASTM A312 304H

ASTM A312 TP304H Chemical Requirements:  Composition, %, max Grade TP304H(S30409) Carbon 0.04-0.10 Manganese 2.00 Phosphorus 0.045 Sulfur 0.030 Silicon 1.00 Chromium 18.0-20.0 Nickel 8.0-11.0   Heat Treating Temperature:  Cold finished 1900 °F [1040 °C] Hot finished 1900 °F [1040 °C]   Tensile Requirements: Tensile Strength, min ksi [MPa] 75 [515] Yield Strength, min ksi [MPa] 30…

ASTM A312 TP304L

ASTM A312 TP304L Chemical Requirements:  Composition, %, max Grade TP304L(S30403) Carbon 0.035 a Manganese 2.00 Phosphorus 0.045 Sulfur 0.030 Silicon 1.00 Chromium 18.0-20.0 Nickel 8.0-13.0 a For small diameter or thin walls or both, where many drawing passes are required, a carbon maximum of 0.040 % is necessary in grades TP304L and TP316L. Small outside diameter tubes…

ASTM A312 TP304

ASTM A312 TP304 Chemical Requirements:  Composition, %, max Grade TP304(S30400) Carbon 0.08 Manganese 2.00 Phosphorus 0.045 Sulfur 0.030 Silicon 1.00 Chromium 18.0-20.0 Nickel 8.0-11.0   Heat Treating Temperature: 1900 °F [1040 °C] Tensile Requirements: Tensile Strength, min ksi [MPa] 75 [515] Yield Strength, min ksi [MPa] 30 [205] Elongation in 2 in. or 50 mm (or 4D),…

BS3692:2001

BS 3692:2001 ISO metric precision hexagon bolts, screws and nuts – Specification BS3692 gives the general dimensions and tolerances of precision hexagon bolts, screws and nuts with ISO metric threads in diameters from 1.6mm to 68mm inclusive. Mechanical properties are given only in respect of carbon or alloy steel bolts, screws and nuts, which are not…

30ХГСА-GOST 4543

Standard: GOST 4543 Steel Grade: 30ХГСА Chemical Requirements  Composition, max, % Elements 30ХГСА Carbon 0.28-0.34 Silicon 0.90-1.20 Manganese 0.80-1.10 Chromium 0.80-1.10 Phosphorus 0.025 Sulfur 0.025 Copper 0.30 Nickel 0.30   Tensile, Impact and Hardness Requirements Steel Grade 30ХГСА Yield Strength, min, N/mm2 835 Ultimate Strength,min, N/mm2 1080 Elongation, min, % 10 Contraction, min, % 45 Shock viscosity…

INCONEL® 625

INCONEL® 625 is a nonmagnetic, corrosion and oxidation resistant, nickel-base alloy. It has high strength and toughness in the temperature range cryogenic to 2000°F (1093°C) which is derived largely from the solid solution effects of the refractory metals, columbium and molybdenum, in a nickel-chromium matrix. Alloy 625 has excellent fatigue strength and stress-corrosion cracking resistance…

40X GOST 4543

Standard: GOST 4543 Steel Grade: 40X Chemical Requirements  Composition, max, % Elements 40X – GOST 4543 Carbon 0.36 – 0.44 Silicon 0.17 – 0.37 Manganese 0.50 – 0.80 Chromium 0.80 – 1.10 Phosphorus 0.035 Sulfur 0.035 Copper 0.30 Nickel 0.30   Tensile, Impact and Hardness Requirements Steel Grade 40X – GOST 4543 Yield Strength, min,…

GOST 4543

GOST 4543 Alloyed Construciton Steel Gost 4543 applies to alloyed construction hot-rolled and forged gauged steel with diameter or thickness up to 250 mm, and steel with a special surface finish, used in a thermally treated condition and produced in the form of bars, strips and hanks. Regarding the standards for chemical composition this Standard…