ASTM A312 TP316L
Chemical Requirements: Composition, %, max
Grade | TP316L(S31603) |
Carbon | 0.035 a |
Manganese | 2.00 |
Phosphorus | 0.045 |
Sulfur | 0.030 |
Silicon | 1.00 |
Chromium | 16.0-18.0 |
Nickel | 11.0-14.0 |
Molybdenum | 2.00-3.00 |
a For small diameter or thin walls or both, where many drawing passes are required, a carbon maximum of 0.040 % is necessary in grades TP304L and TP316L. Small outside diameter tubes are defined as those less than 0.500 in. [12.7 mm] in outside diameter and light wall tubes as those less than 0.049 in. [1.20 mm] in average wall thickness (0.044 in. [1.10 mm] in minimum wall thickness).
Heat Treating Temperature: 1900 °F [1040 °C]
Tensile Requirements:
Tensile Strength, min ksi [MPa] | 70 [485] |
Yield Strength, min ksi [MPa] | 25 [170] |
Elongation in 2 in. or 50 mm (or 4D), min, %:
Longitudinal | 35 |
Transverse | 25 |