ASTM A 312 Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes
UNS Designation N08904
Chemical Requirements: Composition, %, max
C: 0.020
Mn:2.00
P: ≤0.040
S: ≤0.030
Si: 1.00
Cr: 19.0-23.0
Ni:23.0-28.0
Mo: 4.0-5.0
N: 0.10
Cu: 1.00-2.00
Heat Treating Temperature: 1100 °C
Tensile Requirements
Tensile Strength, min.: 490MPa
Yield Strength, min.: 215MPa
Elongation in 2 in. or 50 mm (or 4D), min, %:
Longitudinal 35
Transverse 25