10CrMo9-10

BS EN 10253-2:2007 Butt-welding pipe fittings — Part 2: Non alloy and ferritic alloy steels with specific inspection requirements

Steel grade: 10CrMo9-10

 

Heat treatment condition: NT (Normalized and tempered)

it may be necessary in the case of wall thickness T above 25 mm or T/D > 0,15 to apply quenching and tempering in order to achieve the intended structure and material properties. The decision shall be left to the discretion of the manufacturer but shall be stated to the customer at the time of enquiry and order. Steel tubes treated in such a way shall be designated by the steel name supplemented by the symbol “ +QT”.

Chemical composition

C: 0.08-0.14

Si: ≤0.50

Mn: 0.30-0.70

P: ≤0..025

S: ≤0..020

Al tot: ≤0..040

Cr: 2.0-2.5

Cu: ≤0.30

Mo: 0.90-1.10

Ni: ≤0.30

 

Mechanical properties

Yield strength min. N/mm2

T ≤ 4040 < T ≤ 60
280270

Tensile strength Rm N/mm2:   480-630

Elongation A min. %

LongitudinalTransverse
2220

 

Impact properties

Minimum average absorbed energy KV, in J at a temperature of 20 °C

LongitudinalTransverse
4027