Class60/Class70 – ASTM A181

ASTM A181 – Carbon Steel Forgings, for General-Purpose Piping

Grade: Class60 and Class70

Chemical Requirements  max,%

ElementsClasses 60 and 70
Carbon0.35
Manganese1.10A
Phosphorus0.05
Silicon0.10-0.35
Sulfur0.050

A Manganese may be increased to 1.35 % max provided the carbon is reduced 0.01 % for each 0.06 % increase in manganese over the limit shown in the table.

 

Tensile Requirements

Class 60Class 70
Tensile strength, min, ksi [MPa]60 [415]70 [485]
Yield strength,A min, ksi [MPa]30 [205]36 [250]
Elongation in 2 in. [50 mm], min, %2218
Reduction of area, min, %3524

A Determined by either the 0.2 % offset method or the 0.5 % extension-underload method.