ASTM A182 – Forged or Rolled Alloy and Stainless Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service
Grade: F904L Austenitic Stainless Steel
Chemical Requirements max, %
Elements | F904L(N08904) |
Carbon | 0.020 |
Manganese | 2.00 |
Phosphorus | 0.040 |
Sulfur | 0.030 |
Silicon | 1.00 |
Nickel | 23.0-28.0 |
Chromium | 19.0-23.0 |
Molybdenum | 4.0-5.0 |
Copper | 1.00-2.00 |
Nitrogen | 0.10 |
Tensile and Hardness Requirements
Grade Symbol | F904L(N08904) |
Tensile Strength,min, ksi [Mpa] | 71[490] |
Yield Strength, min,ksi [MPa] | 31[215] |
Elongation in 2 in.[50 mm] or 4D,min, % | 35 |
Reduction of Area, min, % | … |
Brinell HardnessNumber | … |